Corrosion & Salt Spray Testing ASTM B117 Salt Spray (Fog) Testing for Corrosion ResistanceASTM B368 Cyclic Corrosion Testing for CoatingsASTM D1654 Evaluation of Painted or Coated Specimens Subjected to CorrosionASTM D3359 Adhesion Testing of Coatings (Cross-cut)ASTM D4541 Pull-Off Adhesion TestingASTM D610 Evaluation of Rusting on Painted Steel SurfacesASTM D610 Rust Grade RatingASTM D714 Blistering Evaluation on CoatingsASTM D714 Blistering Test for Paints and CoatingsASTM G1 Preparation of Metal Surfaces for Corrosion TestingASTM G101 Environmental Stress Cracking TestingASTM G109 Cathodic Disbondment TestingASTM G110 Corrosion Fatigue Crack GrowthASTM G123 Corrosion in Marine EnvironmentsASTM G123 Corrosion of Stainless Steel in Marine EnvironmentsASTM G129 Corrosion Testing in Chloride EnvironmentsASTM G142 Hydrogen Evolution MeasurementASTM G150 Electrochemical Noise MeasurementsASTM G170 Standard Practice for Testing Materials in CO2 EnvironmentsASTM G192 Evaluation of Corrosion Product FormationASTM G199 Corrosion Testing Under Cathodic ProtectionASTM G28 Laboratory Evaluation of the Corrosivity of SoilASTM G31 Immersion Corrosion TestingASTM G31 Laboratory Corrosion Testing of MetalsASTM G36 Hydrogen Embrittlement TestingASTM G36 Hydrogen Embrittlement TestsASTM G44 Cyclic Corrosion TestingASTM G46 Evaluation of Corrosion Under CoatingsASTM G46 Evaluation of Localized CorrosionASTM G49 Stress Corrosion Cracking Tests in MetalsASTM G5 Anodic Polarization TestingASTM G5 Potentiodynamic Polarization CurvesASTM G59 Electrochemical Impedance Spectroscopy (EIS)ASTM G61 Sulfide Stress Cracking TestingASTM G71 Preparation of Corrosion Testing SolutionsASTM G71 Preparation of Electrolytes for Corrosion TestingASTM G72 Hydrogen EmbrittlementASTM G78 Pitting Corrosion TestingASTM G85 Annex A Acidified Salt Spray (Fog) TestingASTM G85 Annex B Seawater Acidified TestASTM G85 Annex C Cyclic Acidified Salt SprayASTM G85 Annex D Seawater Spray TestASTM G85 Annex E Combined Salt Spray and SO2 ExposureASTM G85 Annex F Acidified Synthetic Seawater SprayASTM G85 Annex G Cyclic Prohesion TestASTM G85 Modified Salt Spray TestingASTM G94 Corrosion Testing of TitaniumASTM G95 Corrosion Fatigue TestingISO 11314 Stress Cracking TestingISO 11462 Electrolyte PreparationISO 11462 Preparation of Test SolutionsISO 11463 Anodic Polarization CurvesISO 11463 Corrosion Testing of Metals by Potentiodynamic PolarizationISO 11463 Potentiodynamic TestingISO 11960 Titanium Corrosion TestingISO 15156 Corrosion in Chloride EnvironmentsISO 15156 Corrosion Testing in CO2 EnvironmentsISO 15589-1 Cathodic Protection TestingISO 16701 Cyclic Corrosion TestingISO 16701 Cyclic Corrosion Testing of CoatingsISO 16773 Electrochemical Impedance Spectroscopy for CorrosionISO 17074 Hydrogen Gas EvolutionISO 17075 Soil Corrosion TestingISO 17475 Electrochemical Testing of CorrosionISO 17475 Immersion TestingISO 17864 Corrosion Rate MeasurementISO 17872 Pitting Corrosion ResistanceISO 17941 Electrochemical Noise AnalysisISO 20340 Corrosion Under Coating EvaluationISO 21809-2 Testing of Anti-corrosion CoatingsISO 2409 Paint Adhesion TestingISO 4624 Adhesion of CoatingsISO 4628-2 Blistering in CoatingsISO 4628-2 Blistering Test for CoatingsISO 4628-3 Rust EvaluationISO 4628-3 Rust Grade AssessmentISO 4628-8 Assessment of Filiform CorrosionISO 4628-8 Evaluation of Degradation of Coatings – Filiform CorrosionISO 6988 Neutral Salt Spray TestISO 7539-2 Stress Corrosion CrackingISO 7539-2 Stress Corrosion Cracking TestingISO 7539-4 Hydrogen Embrittlement TestingISO 7539-5 Slow Strain Rate TestingISO 7539-6 Sulfide Stress CrackingISO 7539-7 Crack Growth TestingISO 7539-8 Corrosion FatigueISO 7539-9 Testing of Stainless Steel CorrosionISO 8407 Surface Preparation for Corrosion TestingISO 9223 Corrosion Rates in Atmospheric EnvironmentsISO 9227 Annex B for Modified Salt SprayISO 9227 Annex C Cyclic Salt SprayISO 9227 Annex D Seawater SprayISO 9227 Annex E Combined Corrosion TestingISO 9227 Annex F Acidified Seawater SprayISO 9227 Annex G Prohesion Corrosion TestingISO 9227 Annexes for Modified Salt SprayISO 9227 Corrosion Tests in Artificial Atmospheres – Salt Spray Tests

ISO 17872 Pitting Corrosion Testing: A Laboratory Testing Service Provided by Eurolab

ISO 17872 Pitting Corrosion Testing is a laboratory testing service that evaluates the resistance of materials to pitting corrosion. This standard is governed by various international and national standards, including ISO, ASTM, EN, TSE, and others.

International Standards:

  • ISO 17872:2015 - Metallic materials - Determination of resistance to pitting corrosion
  • ASTM G150-15 - Standard Test Method for Measurement of Resistance to Pitting Corrosion by Immersion in Sodium Chloride Solution
  • EN ISO 17872:2015 - Metallic materials - Determination of resistance to pitting corrosion
  • National Standards:

  • TSE (Turkish Standards Institution) TS EN ISO 17872:2015 - Metallic materials - Determination of resistance to pitting corrosion
  • Standard Development Organizations:

    The International Organization for Standardization (ISO), the American Society for Testing and Materials (ASTM), and the European Committee for Standardization (CEN) are some of the standard development organizations responsible for creating and maintaining standards related to ISO 17872 Pitting Corrosion Testing.

    Evolution of Standards:

    Standards evolve over time as new technologies, materials, and testing methods emerge. Updates to standards ensure that they remain relevant and effective in evaluating material properties.

    Standard Numbers and Scope:

  • ISO 17872:2015 - Metallic materials - Determination of resistance to pitting corrosion
  • Scope: This standard specifies a method for determining the resistance of metallic materials to pitting corrosion by immersion in sodium chloride solution.

    Purpose: To evaluate the pitting corrosion behavior of metallic materials.

    Compliance Requirements:

    Industry sectors that require compliance with ISO 17872 Pitting Corrosion Testing standards include:

  • Aerospace
  • Automotive
  • Chemical Processing
  • Construction
  • Energy Generation and Storage
  • Why this Test is Needed and Required:

    ISO 17872 Pitting Corrosion Testing is necessary for industries that require high-performance materials with excellent resistance to corrosion. This test ensures that materials meet specific requirements, reducing the risk of pitting corrosion and associated failures.

    Business and Technical Reasons for Conducting ISO 17872 Pitting Corrosion Testing:

  • To evaluate material performance in corrosive environments
  • To ensure compliance with regulatory standards and industry specifications
  • To minimize the risk of equipment failure and downtime
  • To optimize material selection and reduce costs
  • Consequences of Not Performing this Test:

    Failure to conduct ISO 17872 Pitting Corrosion Testing can lead to:

  • Equipment failures due to pitting corrosion
  • Reduced product lifespan and performance
  • Increased maintenance and repair costs
  • Environmental damage from corrosive materials
  • Industries and Sectors that Require this Testing:

    Aerospace, automotive, chemical processing, construction, energy generation and storage, and oil and gas are some of the industries that require ISO 17872 Pitting Corrosion Testing.

    Risk Factors and Safety Implications:

    Pitting corrosion can lead to catastrophic failures, resulting in:

  • Loss of life
  • Environmental damage
  • Economic losses
  • Quality Assurance and Quality Control Aspects:

    ISO 17872 Pitting Corrosion Testing is an essential quality control measure that ensures materials meet specific requirements.

    How this Test Contributes to Product Safety and Reliability:

    By evaluating material resistance to pitting corrosion, ISO 17872 Pitting Corrosion Testing helps ensure product safety and reliability.

    Competitive Advantages of Having this Testing Performed:

    Performing ISO 17872 Pitting Corrosion Testing provides a competitive advantage by:

  • Ensuring compliance with regulatory standards
  • Reducing the risk of equipment failure and downtime
  • Optimizing material selection and reducing costs
  • Cost-Benefit Analysis of Performing this Test:

    While performing ISO 17872 Pitting Corrosion Testing may incur costs, it can provide significant benefits in terms of reduced equipment failures, downtime, and environmental damage.

    Step-by-Step Explanation of How the Test is Conducted:

    1. Sample preparation

    2. Equipment setup and calibration

    3. Testing environment control

    4. Immersion of samples in sodium chloride solution

    5. Measurement and analysis of corrosion rates

    Testing Equipment and Instruments Used:

  • Autoclave or pressure vessel for testing
  • pH meter and temperature controller
  • Corrosion measurement equipment (e.g., electrochemical impedance spectroscopy)
  • Data acquisition and analysis software
  • Testing Environment Requirements:

    Temperature: 35C 2C

    Humidity: 65 5

    Pressure: Atmospheric

    Sample Preparation Procedures:

  • Material selection and procurement
  • Sample cutting and polishing
  • Cleaning and surface preparation
  • Measurement and Analysis of Corrosion Rates:

    Corrosion rates are measured using electrochemical impedance spectroscopy (EIS) or other relevant methods.

    Testing Methodology:

    The testing methodology involves immersing samples in a sodium chloride solution for a specified period, measuring corrosion rates, and analyzing the results.

    Test Results and Reporting:

    Test results are reported as corrosion rates, with specific requirements outlined in industry standards and specifications.

    Conclusion:

    ISO 17872 Pitting Corrosion Testing is an essential laboratory testing service that evaluates material resistance to pitting corrosion. By understanding standard-related information, standard requirements and needs, test conditions and methodology, and the benefits of performing this test, industries can ensure compliance with regulatory standards, reduce equipment failures and downtime, and optimize material selection and costs.

    Eurolabs ISO 17872 Pitting Corrosion Testing Service:

    As a leading laboratory testing service provider, Eurolab offers comprehensive ISO 17872 Pitting Corrosion Testing services, including sample preparation, testing, measurement, analysis, and reporting. Our experienced team ensures accurate and reliable results, helping industries meet regulatory standards and optimize material selection.

    Eurolabs Capabilities:

  • Comprehensive testing services for a wide range of materials
  • State-of-the-art equipment and facilities
  • Experienced team with expertise in corrosion testing
  • Accurate and reliable test results
  • Conclusion:

    By partnering with Eurolab for ISO 17872 Pitting Corrosion Testing, industries can ensure compliance with regulatory standards, reduce the risk of equipment failure and downtime, and optimize material selection and costs. Our comprehensive testing services and expert team help industries achieve their goals and improve overall performance.

    Need help or have a question?
    Contact us for prompt assistance and solutions.

    Latest News

    View all

    JOIN US
    Want to make a difference?

    Careers